铁艺大门表面如何处理?

来源:http://www.jnghbxg.com 日期:2020-11-20 发布人: 浏览次数:45
铁艺大门表面如何处理,下面就请济南铁艺大门为我们讲解一下吧!
How to deal with the surface of iron gate, please explain it to us!
一、焊渣 铁艺大门的焊接部位较多,必须认真每个焊接部位的焊渣。先用板锉或扁铁敲打除渣,然后用磨光机和砂布打磨焊缝,使其平滑。对飞溅到其他部位的焊渣也要顺势干净。
1、 There are many welding parts in the iron gate to remove welding slag, so the welding slag of each welding part must be removed carefully. First, use a plate file or flat iron to knock off the slag, and then use a polishing machine and abrasive cloth to polish the weld to make it smooth. The welding slag splashed to other parts should also be removed.
二、涂抹原子灰 用原子灰加固化剂(比例50:1)搅拌均匀,涂抹在焊接部位.处理焊缝缺陷。
2、 Apply putty with putty and curing agent (proportion 50:1), mix evenly, smear on the welding position, and deal with weld defects.
三、打磨原子灰 干透后,用磨光机和砂布打磨大门的各个组件,尤其是涂抹原子灰的部位更要磨光。
3、 After the putty is completely dry, use a polishing machine and abrasive cloth to polish all components of the gate, especially the parts coated with putty.
 
四、喷漆 喷漆前,用湿布擦净大门的各个部位,不能留有灰尘等。道喷防锈漆,漆膜干透后喷第二道黑漆,后喷一道清漆。注意不能有漏喷部位,也不能产生流挂等缺陷。个别细微处可用刷子刷涂补漆。
4、 Before spray painting, wipe all parts of the gate with a wet cloth, and there should be no dust left. After the film is dry, spray the second layer of black paint, and then spray a layer of varnish. Attention should be paid to no leakage or sagging. Some tiny parts can be applied with brush.
通过以上的讲解,相信大家对铁艺大门表面如何处理有了一定的了解,如果想要深入了解,请关注我们的官网:http://www.jnghbxg.com
Through the above explanation, I believe you have a certain understanding of how to deal with the surface of the iron gate. If you want to know more about it, please pay attention to our official website: http://www.jnghbxg.com